- Other Plastic Products[10]
- Water Treatment[10]
- Plastic Processing Machinery Parts[2]
- Other Metals & Metal Products[2]
- Other Steel Products[5]
- Ceramics[10]
- Chemical Auxiliary Agent[10]
- Exhaust System[2]
- Other Environmental Products[5]
- Other Electronic Components[1]
- Gas Disposal[2]
- Cast & Forged[1]
- Organic Fertilizer[7]
- Contact Person : Ms. Peng Emily
- Company Name : Pingxiang Zhongying Packing Co., Ltd.
- Tel : 0086-799-6812817
- Fax : 0086-799-6812817
- Address : Jiangxi,Pingxiang,No. 14, Zhenxing Lane, Beiqiao Village, Jiaoqu Xiang, Anyuan Dist.
- Country/Region : China
- Zip : 337000
Ceramic saddles packing
Performance features and uses:
Ceramic Intalox saddle has excellent acid resistance and heat resistance. It can resist to corrosion of various inorganic acids, organic acids and organic solvents except hydrofluoric acid, and can be used in high or low temperature conditions. Consequently the application range is very wide. It can be used in the drying columns, absorbing columns, cooling towers, scrubbing towers in chemical industry, metallurgy industry, coal gas industry, oxygen producing industry, etc.....
Ceramic Intalox saddle is the opening packing with the structure of groove hemicycle, which reduce the cover between the packing and enlarge the space, therefore, the availability of the mass transfer surface will be enhanced efficiently, and it has favorable liquid distributing capability.
...
Technical data of the Ceramic Intalox Saddle:
Specification (mm) | Bulk density (kg/m³) | Surface area (m²/m³) | Void space(%) | Number per m³ | Packing factor(m-1) | |
12 | 720 | 623 | 71.7 | 748000 | 200 | |
19 | 688 | 334 | 73 | 310510 | 130 | |
25 | 688 | 253 | 73 | 84600 | 85 | |
38 | 640 | 164 | 75 | 21000 | 50 | |
50 | 577 | 115 | 77.4 | 9400 | 37 | |
76 | 623 | 92 | 75.5 | 2800 | 24 | |
Note: The above data is for reference only. |
Thermal shock test for Intalox SaddlesFor example shipping the saddles over 80 M3:1) Randomly pick 100-200 pieces of ceramic saddles for RTOs from the batch or shipment2) For each sample selected, heat it up to 820 and maintain them at this temperature for 30 minutes.3) Drop the hot pieces into cold 20 water4) Repeat steps 2 & 3 for10 times on each and every piece in the sample lot. 5) Examine the pieces and count the percent that show clear signs of breakage and/or cracking. Our standard is less than seven (7%) percent.
Ceramic saddles packing